On November 6, 2026, the New York State Energy Research and Development Authority (NYSERDA) announced a $250,000 grant to the startup InfinitEnergy for solid-state battery development. The company aims to build a battery that combines high energy density with long cycle life without applying external mechanical pressure during charging and discharging. Syracuse University also highlighted the award on November 20, describing it as an effort to move research results toward commercial use. Solid-state batteries sometimes require applied pressure to keep electrodes and electrolytes in contact, but materials and cell design can also help maintain that contact. Below, we look at the current state of technology for reducing external pressure, based on earlier research and its test conditions.

AD

Why solid-state batteries need pressure

The grant to InfinitEnergy is part of a program supporting the development and demonstration of energy storage technologies before commercialization. NYSERDA is providing about $13 million in total to 15 projects, of which $250,000 goes to the company. The funding program supports technology development and demonstration in New York State, with needs such as meeting peak electricity demand in mind.

InfinitEnergy's co-founders are Quinn Qiao and Anthony Terrinoni. At Syracuse University, Qiao leads the mechanical and aerospace engineering department, and Terrinoni is also affiliated with it. In a university announcement, Qiao said the grant would help turn laboratory results into practical applications.

When gaps form between a solid electrolyte and an electrode, the contact area through which lithium ions can move shrinks, and current tends to concentrate locally even when the same total current is passed. Clamping a stacked cell in the thickness direction helps maintain contact between the electrode and the electrolyte. The pressure applied in this way is called stack pressure. Silicon anodes expand and contract as the battery charges and discharges, and in lithium metal anodes, the loss of lithium during discharge can leave voids at the interface with the solid electrolyte.

However, adding a pressurizing mechanism increases the weight and volume of the battery pack. Even if the cell stores the same amount of energy, the energy density per unit mass or volume of the whole pack goes down. Research that raises the energy density of electrode materials and research that reduces pressurizing hardware are different approaches to improving energy density at the pack level.

A 2022 peer-reviewed paper in ACS Applied Energy Materials by Baniya et al., with Qiao as corresponding author, reported another way to improve the electrode–electrolyte interface. The team placed a thin silicon nitride film between lithium metal and a garnet-type solid electrolyte and measured resistance in symmetric cells with identical lithium metal electrodes on both sides. The area-normalized interfacial resistance on one side fell from 1197 Ω·cm² to 84.5 Ω·cm². In the full-cell tests that combined a cathode and an anode, the team used a hybrid configuration in which a small amount of organic liquid electrolyte was added on the cathode side.

Cells that need no external pressure still have internal pressure

In 2024, Hui Pan and colleagues at Nanjing University reported in a peer-reviewed paper in Nature Communications how they built and evaluated cells that combine a silicon anode with an elastic electrolyte and operate without additional external pressure. In their method, an electrolyte precursor is infiltrated into an anode containing micron-sized silicon particles and cured in place. The electrolyte surrounding the particles follows the volume changes during charging and discharging, maintaining contact with the active material.

Pan and colleagues also built thin sensors into the cell to measure the pressure remaining inside. Internal pressure was 546 kPa in coin cells and 52 kPa in pouch cells, which have a bag-like casing. The cells use internal pressure generated by sealing and cell structure, without extra pressure applied from outside. In this way, pressure applied by an external mechanism must be distinguished from pressure generated inside the cell.

Battery performance was also evaluated for each cell format. A coin-type full cell combining a silicon anode with a lithium iron phosphate cathode retained 98.3% of its capacity after 100 cycles. A separate pouch-type full cell using the same materials delivered a discharge capacity of 11.7 mAh at a low charge-discharge rate of 0.1 C, which corresponds to 140 mAh/g based on the mass of the cathode active material.

However, this 140 mAh/g figure is a specific capacity based on the mass of the cathode active material, not the energy density of the whole cell. To obtain the cell's energy density per unit mass, the electrical energy calculated from discharge voltage and current must be divided by the mass of the entire cell, including the electrolyte and casing. The metrics for evaluating active material performance and real-world battery performance are different.

AD

Interface shape and temperature affect performance at low pressure

In a peer-reviewed paper published in Nature Energy on November 23, Shengming Zhang and colleagues at the University of Oxford reported a method of giving the interface between lithium metal and the sulfide solid electrolyte Li₆PS₅Cl an egg-carton-like textured structure. If the surrounding lithium metal cannot deform fast enough to fill gaps as lithium is lost during discharge, the contact area between electrode and electrolyte shrinks. The team compared the textured samples with ones that have a flat interface to examine how well the texture suppresses void growth.

In three-electrode cells with the textured interface, the upper limit of the current density at which stable discharge could be repeated at a stack pressure of 0.1 MPa was 0.5 mA/cm² at 30°C but rose to 4 mA/cm² at 60°C. In Figures 3c and 3d of the paper, the areal capacity per half cycle is fixed at 1 mAh/cm², and the current density for depositing lithium during charging at 0.2 mA/cm². The charging current density was kept low, so the reported upper limits reflect repeated discharge under this charging condition and areal capacity.

The three-electrode cells add a reference electrode to measure voltage changes on the anode side separately. The team also tested full cells that combine a cathode and an anode. A full cell with the textured structure could be cycled stably at a stack pressure of 2 MPa, a temperature of 60°C and a discharge current density of 6 mA/cm².

The pressure needed during charging and discharging also differs from the pressure needed in manufacturing. Zhang and colleagues applied 400 MPa from one direction during the forming step that densifies the solid electrolyte powder and transfers the textured structure to the interface. Even a cell that operates at low stack pressure may rely on a high-pressure forming process to create its interface structure.

What data is needed to evaluate InfinitEnergy's technology

NYSERDA and Syracuse University have not disclosed the electrode and electrolyte compositions, cell format or capacity of the batteries InfinitEnergy is developing. Data on whole-cell energy density and on cycle life, including charge-discharge conditions, has not been published, and the internal pressure during operation and the manufacturing scale are unknown. It is also unclear whether the company will use the interlayer technologies Qiao has studied previously in this development.

Prior studies report how materials and interface shapes were engineered to maintain electrode–electrolyte contact, along with the pressure and temperature used in testing. For InfinitEnergy as well, performance data for the same cell configuration will be needed, with operating pressure, temperature, current density and charge-discharge capacity stated explicitly. Whole-cell energy density per unit mass, together with capacity retention over repeated cycling, would allow evaluation of the company's two goals of high energy density and long life.

If the pressure needed in manufacturing and the specifications of the restraint hardware needed during operation are also disclosed, the battery's performance as a pack can be assessed. How much weight and volume can be saved by eliminating external pressure depends on the pack-level energy density per unit mass and volume, including the restraint hardware.