A research team led by Wang Hui and Zheng Fangcai at the Hefei Institutes of Physical Science, Chinese Academy of Sciences, has reported a new atomic-level design for an aluminum (Al) single-atom catalyst used in the cathode of sodium-sulfur (Na-S) batteries. Of the four oxygen atoms surrounding each Al atom, one is replaced with nitrogen to promote sulfur reactions. The peer-reviewed paper was first published online on September 16, 2026.
The study targets a cathode that combines sulfur with a catalyst in which Al is dispersed atom by atom. In Na-S batteries, the migration of reaction intermediates during charging and discharging, along with slow sulfur reaction kinetics, limits performance. The team sought to address both problems by changing the "coordination," meaning the types and arrangement of atoms bonded to a metal atom.
According to the paper's published abstract, the newly developed Al–O3N–C/S cathode retained a capacity of 1196 mAh/g after 100 charge-discharge cycles at 0.1 C. A 2500-cycle long-term test is also reported, but the 1196 mAh/g figure was measured after 100 cycles, not after 2,500. The study adopts a coordination structure different from the one in the calcium catalyst the same group developed earlier.
Swapping in nitrogen to tune the Al reaction site
During charging and discharging in a Na-S battery, sulfur reacts with sodium to form sodium polysulfides, which contain multiple sulfur atoms. Some of these dissolve into the electrolyte and travel between the cathode and anode, causing capacity loss. Known as the "shuttle effect," this is one of the main challenges for room-temperature Na-S batteries. The sulfur redox reactions themselves are also slow, so the goal is to speed up the reactions while suppressing the movement of intermediates.
The researchers focused on single-atom catalysts, in which metal atoms are dispersed individually and each serves as a reaction site. According to the institute's announcement, conventional Al single-atom catalysts have an Al–O4 structure, in which four oxygen atoms coordinate to one Al atom. In this study, one of those oxygen atoms was replaced with nitrogen, creating an Al–O3N structure in which three oxygen atoms and one nitrogen atom surround the Al. This makes the in-plane coordination around the Al atom asymmetric.
The catalyst anchored on carbon is denoted Al–O3N–C, and the cathode combining it with sulfur is denoted Al–O3N–C/S. What was replaced is not the Al atom itself but the atoms bonded to it. The design adjusts the electronic state of the metal center and its interaction with sulfur without changing the metal. The battery's basic configuration remains that of a Na-S battery; this is not research on an aluminum-sulfur battery.
Why would swapping one oxygen for nitrogen improve the reactions? According to the abstract of the paper, introducing nitrogen causes "charge localization," a local imbalance in electron distribution, which strengthens the hybridization between Al 3p orbitals and sulfur 3p orbitals. Electron orbitals describe the states of electrons in an atom, and orbital hybridization refers to the interaction between different orbitals. The team explains that these electronic changes suppress the polysulfide shuttle effect and speed up sulfur redox reactions.
In this study, the researchers fabricated the catalyst with the modified coordination structure and measured the battery's capacity. The explanation involving charge localization and orbital hybridization, however, is an interpretation of the reaction mechanism based on electronic structure, and it should be distinguished from the capacity measurements. Changing the coordination structure also does not eliminate every factor that degrades a battery.
How it differs from the earlier calcium study
The approach of introducing nitrogen to tune the catalytic behavior of metal atoms is not new to this study. In 2025, Zheng's group also published research that modified the coordination structure of a calcium (Ca) single-atom catalyst. That paper appeared in Nature Communications, volume 16, article number 4372, with the DOI 10.1038/s41467-025-59437-3.
The main differences between the two studies are the central metal and the position where nitrogen is introduced. The 2025 Ca study modified the axial coordination, whereas the new Al study modifies the in-plane coordination. "Axial" refers to the direction perpendicular to the plane formed by the surrounding atoms, while "in-plane" means along that plane. The structures compare as follows.
| Study | Central metal | Nitrogen position | Change in coordination |
|---|---|---|---|
| 2025 earlier study | Calcium (Ca) | Axial | Axial O in Ca–O5 replaced with N, giving Ca–O4N |
| 2026 current study | Aluminum (Al) | In-plane | One O in Al–O4 replaced with N, giving Al–O3N |
The result is best seen not as the discovery of single-atom catalysts themselves, but as an application of an existing coordination-design strategy to a different metal and a different atomic arrangement. The axial coordination tuning used in the Ca study has been developed into an asymmetric in-plane coordination structure in the Al study. This comparison, however, only organizes the structural differences between the catalysts; it does not indicate which performs better as a battery.
The earlier Ca study evaluated the catalyst structure by X-ray absorption fine structure (XAFS) analysis and investigated the reaction mechanism by combining density functional theory (DFT) calculations with electrochemical measurements. Batteries were evaluated in CR2032 coin cells with a sodium metal anode, measured at 25°C. The electrolyte-to-sulfur ratio was 70 μL/mg, and capacity was calculated based on the mass of sulfur. These measurement conditions were confirmed for the Ca study, and it cannot be assumed that the same conditions applied to the Al study.
The Ca study is also a related earlier work rather than an independent reproduction of the Al catalyst's performance. Within the publicly available materials checked, no report of another research team reproducing the Al results was found.
How to assess 1196 mAh/g and the 2500-cycle test
The reported 1196 mAh/g is the capacity after 100 charge-discharge cycles at 0.1 C. The C-rate indicates the speed of charging and discharging, and mAh/g expresses the electric charge delivered per unit mass. This figure is an experimentally obtained capacity, not a theoretical one. Also, mAh/g, a measure of charge, differs from Wh/kg, a measure of energy density, and the two cannot be directly substituted for each other.
The 2,500 cycles listed in the abstract, meanwhile, refer to the number of cycles in a separate long-term test. Because the C-rate, initial capacity, and final capacity of that test could not be confirmed, capacity retention after 2,500 cycles cannot be calculated from the 1196 mAh/g value after 100 cycles. Nor can the number of cycles alone indicate how many years a product could be used.
The paper, by Fangcai Zheng and colleagues, was published as a Research Article in the peer-reviewed journal Angewandte Chemie International Edition, with the DOI 10.1002/anie.9140872. However, only the published abstract of the original paper could be checked; the full text and supplementary materials were not reviewed. As a result, details such as the number of independent test cells, measurement error, and test temperature are unknown. Along with sulfur loading and electrolyte volume, the exact mass used as the denominator for 1196 mAh/g also could not be confirmed, so it is unclear whether the value is based on sulfur mass alone or on another mass basis.
Comparing the performance of different catalysts and battery configurations requires matching the mass basis for capacity and the charge-discharge rate. In Na-S batteries in particular, the amount of sulfur loaded in the cathode and the amount of electrolyte used change the performance achievable in a practical cell configuration. The reported capacity is a result measured in a research cell, not a figure representing the performance of a commercial cell or a full battery pack.
The researchers cite economic viability and low toxicity as motivations for using main-group metals such as Al as catalysts. However, the choice of catalyst material alone does not determine the manufacturing cost or safety of the entire battery. The published abstract and the institute's announcement contain no specific information on full-battery cost estimates, safety testing, or mass-production processes.
What matters most in this study is that it presents a new coordination design that tunes sulfur reactions by replacing one oxygen atom around an Al atom with nitrogen. Going forward, comparing performance under conditions that specify sulfur loading and electrolyte volume, and obtaining reproduction results from independent research teams, will make it possible to evaluate how much this design contributes to improving battery capacity and durability.